LOCTITE EA 9658.100
Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

Main features
- Non-Woven Glass Film Support
- 177 deg C High-Temperature Cure
- Extended 15-Day Assembly Window
Product Description
LOCTITE EA 9658.100 PSF NWG AERO is the 0.100 lb/sf non-woven glass-supported configuration of a high-temperature epoxy film adhesive for nacelle metal, composite and honeycomb bonding. The film cures for 1 hour at 177 deg C and provides at least 15 days of open assembly time at 25 deg C or 10 days at 32 deg C. Its non-woven glass carrier supports the specified film construction, while controlled flow helps limit hole blockage and excess flash. Refrigerated storage at -18 deg C or below provides a 9-month warranty life.
Key features
- Non-woven glass support: The 0.100 lb/sf NWG configuration uses a non-woven glass fabric carrier.
- High-temperature cure: The film cures for 1 hour at 177 deg C under maintained pressure.
- Extended assembly window: Open assembly time is at least 15 days at 25 deg C or 10 days at 32 deg C.
Applications
Applications include high-temperature nacelle metal, composite and honeycomb bonding where the 0.100 lb/sf NWG configuration is specified.
TDS, SDS & Technical Documents
Technical Specifications
No specifications available.
Additional Information
As-supplied properties
Configuration-specific and common EA 9658 handling values.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Configuration | EA 9658 .100 PSF NWG | Specific product variant | |
| Construction | Non-woven glass supported | NWG film | |
| Standard package | 36 in x 150 ft | 450 sf roll | |
| Open assembly time | At least 15 | days | At 25 deg C |
| Open assembly time | At least 10 | days | At 32 deg C |
| Storage temperature | -18 or below | deg C | Sealed container |
| Warranty life | 9 | months | At -18 deg C or below, from shipment |
| Cure schedule | 1 hour at 177 deg C | Heat-up rate 2.2 to 4 deg C/minute |