LOCTITE EA 9690.060K

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

LOCTITE EA 9690.060K

Main features

  • High-Peel Structural Bonding
  • Knit-Supported Film Handling
  • Sub-121 deg C Cure

Product Description

LOCTITE EA 9690.060K AERO is a 0.060 lb/sf knit-supported modified epoxy film adhesive for aerospace structural bonding. The low-flow film is formulated for metal, composite and honeycomb assemblies that require bond toughness and high peel capability. Its knit carrier supports handling of the specified film construction, and the adhesive cures below 121 deg C. The 36 in by 167 ft roll format supports lay-up in structural panels and sandwich constructions where the .060K grade is specified.

Key features

  • High-peel structural bonding: The modified epoxy system is formulated for tough structural bonds with high peel capability.
  • Knit-supported construction: The 0.060 lb/sf film uses a knit carrier for the specified .060K configuration.
  • Lower-temperature cure: The film cures below 121 deg C.

Applications

Applications include aerospace metal, composite and honeycomb structural bonding where the .060K knit-supported configuration is specified.

Product Family

LOCTITE EA 9690.060K

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
116/93 °C

Additional Information

Technical properties

As-supplied properties

Physical format and supplied configuration.

Property Value Unit Method / condition
ConfigurationEA 9690 .060KSpecific product variant
Film weight0.060lb/sfSupplied film
Support carrierKnittedK configuration
Roll width36inStandard roll
Roll length167ftStandard roll
Roll area501sfPer roll

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers