PERMABOND QFS10
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Main features
- 5-Second Steel Set Time
- Faster Cure Through Gaps
- Porous Surface Activation
Product Description
Permabond QFS10 is a water-white cyanoacrylate activator that accelerates set on porous or poorly mated parts and through sizable gaps. Applied by wiping, spraying, or dipping one component, it must evaporate before cyanoacrylate is placed on the untreated surface. With a 100 cP ethyl-2-cyanoacrylate at 23 deg C, typical set time is 5 seconds on gap-free steel and 40-60 seconds across a 5 mil gap. QFS10 also supports wire tacking, post-application curing of excess fillets, and reduced frosting or fogging on supported assemblies.
Key features
- Faster Gap Cure: Accelerates cyanoacrylate set through poorly mated joints and sizable gaps.
- Porous Surface Activation: Limits adhesive soak-in before cure on porous materials.
- Post-Application Activation: May be sprayed or dripped onto excess fillets and wire-tacking joints.
Applications
Applications include porous-part bonding, poorly mated joints, wire tacking, excess-fillet cure, and supported plastic assemblies.
Technical Specifications
No specifications available.
Additional Information
As supplied / before processing
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Product type | Cyanoacrylate activator | As supplied | |
| Color | Water-white | As supplied | |
| Flash point | -4.4 | deg C | As supplied |
| Application method | Wipe, spray, or dip one component | Allow full evaporation before bonding | |
| Storage temperature | 5 to 25 | deg C | Recommended storage range |
After processing / final state
Set-time values apply to 100 cP ethyl-2-cyanoacrylate at 23 deg C; the control row is identified separately.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Set time - steel, no gap | 5 | seconds | At 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS10 |
| Set time - steel, 5 mil gap | 40-60 | seconds | At 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS10 |
| Set time - steel, no gap, control | 10-15 | seconds | At 23 deg C without QFS10 |
| Set time - Buna-N, no gap | 10 | seconds | At 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS10 |
| Set time - phenolic, no gap | 5 | seconds | At 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS10 |