PLEXUS MA320
Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls

Main features
- Controlled 10-11 Minute Assembly
- Broad 0.75-9.5 mm Gap Range
- Flexible 40-80% Cured Elongation
Product Description
Plexus MA320 is a two-part, 10:1 methacrylate adhesive for structural bonding of thermoplastic, metal, and composite assemblies in transportation, marine, wind-energy, and engineering-construction applications. The non-sagging grade provides a 10-11 minute work time at 75 deg F (23.9 deg C) and a 0.75-9.5 mm gap tolerance. Typical cured properties include 12.4-15.2 MPa tensile strength, 40-80% elongation, and 64 Shore D hardness. The formulation is supplied in white, off-white, or black and provides toughness at low temperatures.
Key features
- 10-11 Minute Work Window: Provides controlled assembly time at 75 deg F (23.9 deg C).
- 0.75-9.5 mm Gap Tolerance: Supports varied structural joint thicknesses.
- 40-80% Cured Elongation: Typical cured elongation is 40-80%.
Applications
Applications include structural bonding in transportation, marine, wind-energy, and engineering-construction assemblies using supported thermoplastics, metals, and composites.
Technical Specifications
No specifications available.
Additional Information
As-supplied / before-processing properties
Values are typical for the separate components and processing at 75 deg F (23.9 deg C) where stated.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Component color - Part A / Part B | Off-white / white | Typical uncured; other supplied colors are listed | |
| Mix ratio by volume | 10:1 | Part A to Part B | |
| Mix ratio by weight | 6.18:1.00 | Part A to Part B | |
| Component density - Part A | 0.92 | g/mL | Typical uncured |
| Component density - Part B | 1.51 | g/mL | Typical uncured |
| Component viscosity - Part A / Part B | 135-175 / 35-70 | x 1,000 cP | Typical uncured |
| Work time | 10-11 | minutes | At 75 deg F (23.9 deg C) |
| Time to 500 psi (3.4 MPa) | 38-40 | minutes | At 75 deg F (23.9 deg C) |
After-processing / final-state properties
Values are typical cured properties; lap-shear results apply only to the stated substrate and test method.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Gap tolerance | 0.75-9.5 | mm | Typical cured joint range |
| Hardness | 64 | Shore D | Typical cured property |
| Tensile strength | 12.4-15.2 | MPa | ASTM D638 / ISO 527 |
| Tensile modulus | 469-634 | MPa | ASTM D638 / ISO 527 |
| Elongation at break | 40-80 | % | ASTM D638 / ISO 527 |
| Lap shear - aluminum | 14.9 | MPa | ASTM D1002; cohesive failure |
| Lap shear - stainless steel | 18.6 | MPa | ASTM D1002; cohesive failure |
| Lap shear - GRP | 14.4 | MPa | ASTM D1002; fiber tear |